Procedure
- Begin heating water to 80°C.
- Add Phase A ingredients one by one, mixing each until uniform.
- Combine Phase B ingredients, and heat to 80–85°C until melted.
- Add Phase B to Phase A under agitation.
- Mix at high speed until emulsion is uniform.
- Final pH should be 6-7 (adjust with TEA if necessary).
- Pour into containers at 55-60°C.
Stability Information
One month at room temperature, one month at 45°C, three freeze/thaw cycles.
Supplier Information
- Koster Keunen, Inc.
- Lubrizol
- Rita
- Brenntag Specialties
- Vantage Chemicals
Ingredient Trade Name |
INCI Name |
% |
---|---|---|
Phase A | ||
Deionized Water | Aqua | 62.55 |
Disodium EDTA | Disodium EDTA | 0.05 |
Pemulan TR-12 | Acrylates/C10-30 Alkyl Acrylate Crosspolymer | 0.1 |
Tealan 993 | Triethanolamine | 0.3 |
Optiphen4 | Phenoxyethanol, Caprylyl Glycol | 1.0 |
Propylene Glycol | Propylene Glycol | 5.0 |
PVP K-904 | PVP | 5.0 |
Phase B | ||
SynKos 20301 | Synthetic Wax | 10.0 |
Synthetic Beeswax 1221 | Synthetic Beeswax | 8.0 |
Kester Wax K-241 | Lauryl Laurate | 4.0 |
Lipomulse 1655 | Glyceryl Stearate (and) PEG-100 Stearate | 4.0 |