Procedure
- Begin heating water to 80°C. Add Phase A ingredients one by one, mixing each until uniform.
- Combine Phase B ingredients, and heat to 80–85°C until melted.
- Add Phase B to Phase A under agitation. Mix at high speed until emulsion is uniform.
- Final pH should be 6–7 (adjust with KOH if necessary).
- Pour into containers at 55–60°C.
Stability Information
Three months at room temperature, three months at 45°C, three freeze/thaw cycles.
Supplier Information
- Koster Keunen, Inc.
- Lubrizol
- Brenntag Specialties
- Jeen International
- Vantage Chemicals
Ingredient Trade Name |
INCI Name |
% |
---|---|---|
Phase A | ||
Deionized Water | Aqua | 71.55 |
Disodium EDTA | Disodium EDTA | 0.05 |
Carbopol 9802 | Carbomer | 0.6 |
KOH 10% solution | Potassium Hydroxide | 1.8 |
Optiphen3 | Phenoxyethanol, Caprylyl Glycol | 1.0 |
Jeechem BUGL4 | Butylene Glycol | 5.0 |
Phase B | ||
SynKos 20301 | Synthetic Wax | 6.0 |
Synthetic Beeswax 1221 | Synthetic Beeswax | 5.0 |
Kester Wax K-241 | Lauryl Laurate | 4.5 |
Lipomulse 1655 | Glyceryl Stearate (and) PEG-100 Stearate | 4.5 |