Procedure
- Combine Phase A ingredients and mix well, while heating to 85-90°C. Homogenize, if necessary, to ensure ZnO is well dispersed.
- Combine Phase B ingredients and heat to 85-90°C.
- Once both Phases are at temperature, add Phase B to Phase A and shear at high speed.
- Cool with propeller mixing to 70-75°C and fill containers, continue agitation throughout filling.
- Allow to cool undisturbed.
Stability Information
Three months at 45°C, three months at room temperature, three freeze/thaw cycles.
Supplier Information
- Koster Keunen, Inc.
- Lanxess
- Jeen
- Grant Inc
- Evonik
- Brenntag Specialties
Ingredient Trade Name |
INCI Name |
% |
---|---|---|
Phase A | ||
Synkos O-10701 | Synthetic Wax | 15.0 |
Kester Wax K-241 | Lauryl Laurate | 3.0 |
Purolan IHD2 | Isohexadecane | 10.0 |
Jeechem IPM3 | Isopropyl Myristate | 3.0 |
UV Cut ZnO-68-CG4 | Zinc Oxide, Caprylic/Capric Triglyceride, Polyhydroxystearic Acid | 36.8 |
Abil EM 1805 | Cetyl PEG/PPG-10/1 Dimethicone | 1.5 |
Kostol PGP1 | Polyglyceryl-3 Stearate, Beheneth-5 | 2.0 |
Phase B | ||
Deionized Water | Aqua | 23.6 |
Optiphen6 | Phenoxyethanol, Caprylyl Glycol | 0.5 |
Jeechem BUGL3 | Butylene Glycol | 3.0 |
Sodium Chloride | Sodium Chloride | 0.8 |
Magnesium Sulfate | Magnesium Sulfate | 0.8 |